Titanium alloys are metals that contain a mixture of titanium and other chemical elements. Such alloys have very high tensile strength and toughness (even at extreme temperatures). They are light in weight, have extraordinary corrosion resistance and the ability to withstand extreme temperatures.
C | .08 max |
N | .03 max |
O | .18 max |
H | .015 max |
Ti | bal |
Fe | .20 max |
SIZE 6MM TO 200MM DIA ROUND BAR.
SIZE 1MM TO 100MM THICKNESS PLATE.
SIZE 6MM TO 350MM OD PIPE AVAILABLE WITH US IN STOCK.
SIZE 0.5MM TO 6MM DIA WIRE.
.AVAILABLE IN STOCK.
Additional Information:
Features
Forgings : AMS 4981, MIL-T-9047
Round Bar : AMS 4981
Titanium mixed with other chemical elements such as aluminum, molybdenum and zirconium produces a wide range of titanium alloys.
Grade 6Al 2Sn 4Zr 6Mo titanium alloy possesses high strength at elevated temperatures, good hardenability and good weldability. It is heat-treatable alpha-beta alloy.
The following sections will discuss grade 6Al 2Sn 4Zr 6Mo titanium alloy in detail.
Chemical CompositionThe chemical composition of grade 6Al 2Sn 4Zr 6Mo titanium alloy is outlined in the following table.
Element | Content (%) |
---|---|
Molybdenum, Mo | 6 |
Aluminum, Al | 6 |
Zirconium, Zr | 4 |
Tin, Sn | 2 |
Titanium, Ti | Balance |
SIZE 6MM TO 200MM DIA ROUND BAR.
SIZE 1MM TO 100MM THICKNESS PLATE.
SIZE 6MM TO 350MM OD PIPE .
SIZE 0.5MM TO 6MM DIA WIRE.
.AVAILABLE IN STOCK.
Additional Information:
Features
Forgings : MIL-T-9046, MIL-T-9047
Round : ASME SB-348, AMS 4957, AMS 4958
Sheet/Plate : ASME SB-265
This metastable beta alloy is strip producible and cold formable. The alloy has been used for springs, fasteners, torsion bars and as extruded tubulars for deep sour well applications and is listed with the MR0175 approved alloys. The alloy is heat treatable to a wide range of strengths.
Beta C Grade 20Grade 20 has identical mechanical and physical properties to Grade 19 but has the addition of palladium (0.04-0.08%) to increase its corrosion resistance in extreme sour environments at elevated temperature.
CompositionTable 1. The composition of Ti3Al8V6Cr4Mo4Zr.
| Content |
C | <0.05% |
N2 | <0.03% |
O2 | <0.14% |
Al | 3.0-4.0% |
V | 7.5-8.5% |
Cr | 5.5-6.5% |
Zr | 3.5-4.5% |
Mo | 3.5-4.5% |
Ti | Balance |
SIZE 6MM TO 200MM DIA ROUND BAR.
SIZE 1MM TO 100MM THICKNESS PLATE.
SIZE 6MM TO 350MM OD PIPE .
SIZE 0.5MM TO 6MM DIA WIRE.
.AVAILABLE IN STOCK.
Additional Information:
Features
Forgings : MIL-T-9046, MIL-T-9047
Round : ASME SB-348, AMS 4930, AMS 4931, AMS 4956
Sheet/Plate : ASME SB-265, ASTM F136, AMS 4907
Titanium alloys are divided into three main groups: alpha-phase, beta-phase, and alpha-beta-phase. Grade 23 Ti 6Al 4V ELI alloy is an alpha-beta wrought alloy. The ELI stands for extra low interstitial. For an alloy to be branded as an ELI product, it should be produced as such at the mill.
The following sections will discuss in detail about grade 23 Ti 6Al 4V ELI alloy.
Chemical CompositionThe chemical composition of grade 23 Ti 6Al 4V ELI alloy is outlined in the following table.
Element | Content (%) |
---|---|
Titanium, Ti | 88.09 - 91 |
Aluminum, Al | 5.5 - 6.5 |
Vanadium, V | 3.5 - 4.5 |
Iron, Fe | ≤ 0.25 |
Carbon, C | ≤ 0.080 |
Nitrogen, N | ≤ 0.030 |
Hydrogen, H | ≤ 0.0125 |
Other, each | ≤ 0.10 |
Other, total | ≤ 0.40 |
SIZE 6MM TO 200MM DIA ROUND BAR.
SIZE 1MM TO 100MM THICKNESS PLATE.
SIZE 6MM TO 350MM OD PIPE .
SIZE 0.5MM TO 6MM DIA WIRE.
.AVAILABLE IN STOCK.
Additional Information:
Table 1. The composition of Ti10V2Fe3Al.
| Content |
C | <0.05% |
N2 | <0.05% |
O2 | <0.13% |
Al | 2.6-3.4% |
Fe | 1.6-2.2% |
V | 9.0-11.0% |
H2 | <0.015%% |
Ti | Balance |
SIZE 6MM TO 200MM DIA ROUND BAR.
SIZE 1MM TO 100MM THICKNESS PLATE.
SIZE 6MM TO 350MM OD PIPE .
SIZE 0.5MM TO 6MM DIA WIRE.
.AVAILABLE IN STOCK.
Additional Information:
Features
Fittings : ASME SB-363
Forgings : ASME SB-381
Pipe : ASME SB-337
Round Bar/Wire : ASME SB-348, ASTM F-67, AMS 4921
Sheet/Plate : ASME SB-265, AMS 4901
Tube : ASME SB-338
CP titanium Grade 4 provides corrosion resistance, strength and fatigue characteristics that compare favorably to those of nickel and steel alloys. The strongest grade of unalloyed grades 1, 2, 3 and 4, this is a commercially pure, moderately formable alloy with good ductility.
CHEMICAL COMPOSITION OF CP TITANIUM GRADE 4SIZE 6MM TO 200MM DIA ROUND BAR.
SIZE 1MM TO 100MM THICKNESS PLATE.
SIZE 6MM TO 350MM OD PIPE .
SIZE 0.5MM TO 6MM DIA WIRE.
.AVAILABLE IN STOCK.
Additional Information:
Fittings : ASME SB-363
Forgings : ASME SB-381
Pipe : ASME SB-337, ASME SB-338
Round Bar/Wire : ASME SB-348,ASTM F-67, AMS 4921
Sheet/Plate : ASME SB-265, AMS 4902
Tube : ASME SB-337, ASME SB-338b, AMS 4942
CP titanium Grade 2 offers excellent corrosion resistance, superior formability and strength between grades 1 and 3. It’s a widely used grade that offers a yield strength of 275MPa (40ksi) minimum.
CHEMICAL COMPOSITION OF CP TITANIUM GRADE 2 – ASTM B 348 (99)
SIZE 6MM TO 200MM DIA ROUND BAR.
SIZE 1MM TO 100MM THICKNESS PLATE.
SIZE 6MM TO 350MM OD PIPE .
SIZE 0.5MM TO 6MM DIA WIRE.
.AVAILABLE IN STOCK.
Features
Fittings : ASME SB-363
Forgings : ASME SB-381
Pipe : ASME SB-337, ASME SB-338
Round Bar/Wire : ASME SB-348
Sheet/Plate : ASME SB-265
Tube : ASME SB-337, ASME SB-338
Component | Wt. % | |
C | Max 0.1 | |
Fe | Max 0.3 | |
H | Max 0.015 | |
N | Max 0.03 | |
O | Max 0.25 | |
Pd | 0.2 | |
Ti | 99 |
SIZE 6MM TO 200MM DIA ROUND BAR.
SIZE 1MM TO 100MM THICKNESS PLATE.
SIZE 6MM TO 350MM OD PIPE .
SIZE 0.5MM TO 6MM DIA WIRE.
.AVAILABLE IN STOCK.
Additional Information:
Features
Features
Forgings : ASME SB-381
Pipe : ASME SB-337
Round Bar : ASME SB-348
Sheet/Plate : ASME SB-265
Tube : AMS 4943, AMS 4944, ASME SB-338
Features
Forgings : MIL-T-9046, MIL-T-9047
Round : AMS 4971, AMS 4978, AMS 4979
Sheet/Plate : AMS 4918
The following table shows the chemical composition of grade 450 stainless steel alloy.
Element | Content (%) |
---|---|
Iron, Fe | 74.3 |
Chromium, Cr | 15 |
Nickel, Ni | 6 |
Copper, Cu | 1.5 |
Silicon, Si | 1.0 |
Manganese, Mn | 1.0 |
Molybdenum, Mo | 0.75 |
Niobium, Nb (Columbium, Cb) | 0.40 |
Carbon, C | 0.050 |
Phosphorous, P | 0.030 |
Sulfur, S | 0.030 |
The physical properties of grade 450 stainless steel alloy are displayed in the following table.
Properties | Metric | Imperial |
---|---|---|
Density | 7.80 cm³ | 0.282 lb/in³ |
The following table outlines the mechanical properties of grade 450 stainless steel alloy.
Properties | Metric | Imperial |
---|---|---|
Tensile strength | 986 MPa | 143000 psi |
Yield strength (@ strain 0.200%) | 814 MPa | 118000 psi |
Bulk modulus (typical for steel) | 166 GPa | 24100 ksi |
Shear modulus (typical for steel) | 83.9 GPa | 12200 ksi |
Charpy impact | 125 - 141 J | 92.2 - 104 ft-lb |
Elongation at break (gage length is 4 times specimen diameter) | 13.30% | 13.30% |
Hardness, Brinell (converted from Rockwell C hardness) | 278 | 278 |
Hardness, Knoop (converted from Rockwell C hardness) | 296 | 296 |
Hardness, Rockwell C | 28 | 28 |
Hardness, Vickers (converted from Rockwell C hardness) | 287 | 287 |
SIZE 6MM TO 200MM DIA ROUND BAR.
SIZE 1MM TO 100MM THICKNESS PLATE.
SIZE 6MM TO 350MM OD PIPE .
SIZE 0.5MM TO 6MM DIA WIRE.
.AVAILABLE IN STOCK.
Additional Information:
The following table shows the chemical composition of grade 450 stainless steel alloy.
Element | Content (%) |
---|---|
Iron, Fe | 74.3 |
Chromium, Cr | 15 |
Nickel, Ni | 6 |
Copper, Cu | 1.5 |
Silicon, Si | 1.0 |
Manganese, Mn | 1.0 |
Molybdenum, Mo | 0.75 |
Niobium, Nb (Columbium, Cb) | 0.40 |
Carbon, C | 0.050 |
Phosphorous, P | 0.030 |
Sulfur, S | 0.030 |
The physical properties of grade 450 stainless steel alloy are displayed in the following table.
Properties | Metric | Imperial |
---|---|---|
Density | 7.80 cm³ | 0.282 lb/in³ |
The following table outlines the mechanical properties of grade 450 stainless steel alloy.
Properties | Metric | Imperial |
---|---|---|
Tensile strength | 986 MPa | 143000 psi |
Yield strength (@ strain 0.200%) | 814 MPa | 118000 psi |
Bulk modulus (typical for steel) | 166 GPa | 24100 ksi |
Shear modulus (typical for steel) | 83.9 GPa | 12200 ksi |
Charpy impact | 125 - 141 J | 92.2 - 104 ft-lb |
Elongation at break (gage length is 4 times specimen diameter) | 13.30% | 13.30% |
Hardness, Brinell (converted from Rockwell C hardness) | 278 | 278 |
Hardness, Knoop (converted from Rockwell C hardness) | 296 | 296 |
Hardness, Rockwell C | 28 | 28 |
Hardness, Vickers (converted from Rockwell C hardness) | 287 | 287 |
SIZE 6MM TO 200MM DIA ROUND BAR.
SIZE 1MM TO 100MM THICKNESS PLATE.
SIZE 6MM TO 350MM OD PIPE .
SIZE 0.5MM TO 6MM DIA WIRE.
.AVAILABLE IN STOCK.
Additional Information:
C | .08 max |
N | .03 max |
O | .25 max |
H | .015 max |
Pd | .12- .25 |
Ti | bal |
Fe | .30 max |
SIZE 6MM TO 200MM DIA ROUND BAR.
SIZE 1MM TO 100MM THICKNESS PLATE.
SIZE 6MM TO 350MM OD PIPE AVAILABLE WITH US IN STOCK.
SIZE 0.5MM TO 6MM DIA WIRE.
.AVAILABLE IN STOCK.
Additional Information: